Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 °C |
27.8 µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000F PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed) |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | TMA |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60 Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 50.0 - 150 °C |
27.8 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
CTE, linear, Transverse to Flow | 50.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |