Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 1.00 - 127 µm/m-°C | 0.556 - 70.6 µin/in-°F | Average value: 101 µm/m-°C Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature 20.0 °C |
0.556 µin/in-°F @Temperature 68.0 °F |
dry |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant. |