Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame retardant. Added features include: Easy Molding, Internally Lubricated, Flame retardant. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East) Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I.. |
|||
CTE, linear, Transverse to Flow | 71.0 - 88.0 µm/m-°C @Temperature 55.0 - 320 °C |
39.4 - 48.9 µin/in-°F @Temperature 131 - 608 °F |
Average value: 84.1 µm/m-°C Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
CTE, linear, Transverse to Flow | 71.0 - 94.0 µm/m-°C @Temperature 55.0 - 320 °C |
39.4 - 52.2 µin/in-°F @Temperature 131 - 608 °F |
Average value: 84.1 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
CTE, linear, Transverse to Flow | 71.0 - 94.0 µm/m-°C @Thickness 2.00 - 4.00 mm |
39.4 - 52.2 µin/in-°F @Thickness 0.0787 - 0.157 in |
Average value: 84.1 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66 LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RFM-3353 EM PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFM-3353 EM is a compound based on Nylon 66 resin containing Glass Fiber, Mineral. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate