Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945 PC Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific) Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat.. |
|||
CTE, linear, Transverse to Flow | 66.6 - 84.6 µm/m-°C @Temperature 100 - 100 °C |
37.0 - 47.0 µin/in-°F @Temperature 212 - 212 °F |
Average value: 75.6 µm/m-°C Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 925 PC Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945U PC (Asia Pacific) Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955 PC Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955 PC (Asia Pacific) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955U PC (Asia Pacific) Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific) Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945 PC (Asia Pacific) Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945W PC (Asia Pacific) Lexan* 945W Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque colo.. |