Polymer Property : CTE, linear, Transverse to Flow = 31.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
17.2 µin/in-°F

@Temperature 73.4 - 131 °F
ASTM E831
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced
Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12
LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers.
CTE, linear, Transverse to Flow 31.0 µm/m-°C
17.2 µin/in-°F
TMA
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Thickness 1.60 mm
17.2 µin/in-°F

@Thickness 0.0630 in
ASTM D696
E-Polymers SEPAZ® K365GM 60% Glass Fiber/Calcium Carbonate Reinforced General Purpose PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..