Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1201-15 Polyester SMC Premi-Glas® 1201-15 is a 15% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 25.0 - 35.0 µm/m-°C @Temperature 20.0 °C |
13.9 - 19.4 µin/in-°F @Temperature 68.0 °F |
|
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | TMA |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |