Polymer Property : Glass Transition Temp, Tg = 302 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 143 - 150 °C
289 - 302 °F
Average value: 145 °C Grade Count:5
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
Average value: 148 °C Grade Count:4
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
Average value: 148 °C Grade Count:5
Overview of materials for Polycarbonate/Styrenic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a..
Glass Transition Temp, Tg 108 - 150 °C
226 - 302 °F
Average value: 136 °C Grade Count:5
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.10% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.