Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
Reliance Industries METABOLIX PHB Information provided by Reliance Industries |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® U1753C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® US230 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
Unitika elitel UE3220 Polyester, Flake Adhesive agent, Resin modifier, Soft type, Standard resinUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a.. |
|||
Glass Transition Temp, Tg | 5.00 - 36.0 °C | 41.0 - 96.8 °F | |
Zeus THV Tubing THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | Ultimate Tg |
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
Hexcel® HexPly® M27 248°F (120°C) Curing Epoxy Matrix HexPly® M27 is specifically designed for applications with fast curing cycles. It is ideally suited for high volume production techniques-in particular for ski manufacture. HexPly® M27 has been sp.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
DSM Biomedical CarboSil® 20 55D Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU) A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th.. |
|||
Glass Transition Temp, Tg | >= 5.00 °C | >= 41.0 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | cond., dynamic; DIN 53 736 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | cond., dynamic; DIN 53 736 |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
Dow Latex LXC 811NA Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 811NA for carpet is a high-performance latex that offers many benefits over standard styrene-butadiene latexes. LXC 811 is a truly unique product that can be used in either r.. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | cond., dynamic; DIN 53 736 |
Hippe PA 6 G Thick-wall pre-forms, heavy semi-finished products. Transfusion of inserts (rolls, cores) and all types of large preforms.Information provided by Hippe. |
|||
Glass Transition Temp, Tg | 5.00 °C | 41.0 °F | |
Atom Adhesives AA-DUCT 916 Epoxy Adhesive AA-DUCT 916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good elect.. |
|||
Glass Transition Temp, Tg | 5.00 - 50.0 °C | 41.0 - 122 °F | Average value: 39.2 °C Grade Count:5 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |