Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 90.0 °C | 194 °F | |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | 10°C/min; DAM; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | Average value: 90.0 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | Average value: 90.0 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | ASTM E1356 |
Solvay Specialty Polymers Hyflon® AD 40L Perfluoropolymer Hyflon® AD 40L is an amorphous perfluoro-polymer available in powder form. Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high t.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | Wet |
Hexcel® HexPly® M10E Epoxy Resin HexPly® M10E is an epoxy resin system preimpregnated into aramid, glass or graphite multiaxial fabrics and unidirectional fibers. M10E prepregs are recommended for the production of low cost, large.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | Ultimate Tg |
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® H37-MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H37-MP is a single component, electrically conductive, thixotropic silver-filled adhesive for die-attach and SMD attach inside hybrid microelectronic packages. Also av.. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope.. |
|||
Glass Transition Temp, Tg | >= 90.0 °C | >= 194 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.Advantages & Application N.. |
|||
Glass Transition Temp, Tg | 90.0 °C | 194 °F | |
Atom Adhesives AA-BOND F110 Epoxy Adhesive AA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. AA-BOND F110 is room temperature system an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
Glass Transition Temp, Tg | 90.0 - 140 °C | 194 - 284 °F | Average value: 123 °C Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and ma.. |