Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lucite International Elvacite ® 4080 Acrylic Resin Elvacite® 4080 is a medium molecular weight methyl methacrylate copolymer. It is a relatively flexible acrylic resin useful for improving the recoatability and intercoat adhesion of UV wood finis.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior .. |
|||
Glass Transition Temp, Tg | 75.0 - 80.0 °C | 167 - 176 °F | |
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 216H02 Opaque Black Epoxy Casting Compound TRA-CAST 216H02 is a medium viscosity two-part formulation recommended for general purpose electrical potting and encapsulation applications where the combination of good mechanical thermal and elec.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE373 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | ASTM D1525 |
Eastman Eastar GN077 Copolyester, Natural Eastar Copolyester GN077 is an amorphous resin with good melt strength, chemical resistance, high clarity and gloss. It is an excellent choice for extrusion blow molding small to intermediate size c.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)
(discontinued **) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |