Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 50.0 °C | 122 °F | ISO 11357-1 |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | ISO 11357-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | ISO 11357-1 |
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
Lucite International Elvacite ® 2045 Acrylic Resin Elvacite® 2045 is a high molecular weight iso-butyl methacrylate polymer. Elvacite® 2045 is useful in topcoats for vacuum metallized plastics and in lacquers for other solvent – sensitive.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | ASTM E1356 |
SK Chemicals SKYTHANE® US210 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg; TMA |
Tra-Con Tra-Bond 546S02 Low Viscosity UV Curable Adhesive TRA-BOND 546S02 is a low viscosity UV curable adhesive exhibiting exceptional adhesion to glass. TRA-BOND 546S02 is designed to be semi-flexible resulting in stress free bonds to glass and other sub.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg |
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg |
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | dry, dynamic; DIN 53 736 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
3M Scotchkote™ 162PWX Epoxy Coating 3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or .. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |
|||
Glass Transition Temp, Tg | 50.0 °C | 122 °F | TM R050-25 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |