Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 5862 Fluoro-silicone Fluoro-siliconeInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7017 Ethylene-Propylene Rubber General service EPM.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7075 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7189 Ethylene-Propylene Rubber General service EPDMInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7204 Ethylene-Propylene Rubber Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7240 Ethylene-Propylene Rubber Potable water service. Chloramine resistant.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7267 Ethylene-Propylene Rubber EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7017 Ethylene-Propylene Rubber General service EPM.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
Seals Eastern 7045 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -51.1 - 3.00 °C | -60.0 - 37.4 °F | Average value: -18.6 °C Grade Count:174 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |