Thermal Properties Metric English Comments
Glass Transition Temp, Tg -47.0 - 120 °C
-52.6 - 248 °F
Average value: -22.9 °C Grade Count:39
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
DSC
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
DSC
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane
Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
Dow Method
Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer
AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be..
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
Pellet sample
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.