Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Multibase Multi-Flex® TPE D 4502 BLK Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Multibase Multi-Flex® TPO D 4508 D 4508 This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Reliance Industries METABOLIX PHO Information provided by Reliance Industries |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | ASTM D3417 |
REXtac Rextac® RT 2880 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point and excellent tensile propertiesApplications: Component of hot melt adhesives, sealants.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | DMTA |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS 440-200 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Mallard Creek Polymers ROVENE® 5044 SBR Latex ROVENE® 5044 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label and construction adhesives. Its relative low molecular w.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Styron Enversaâ„¢ 705A Formulated SB Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Styron XZ 97224.00 Carboxylated SB Performance Features: Good compatibility with natural latex, flexibilityApplications: Leather BindingEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | |
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -35.0 - -25.0 °C | -31.0 - -13.0 °F | |
Zeon Chemicals Nipol® 1432T Nitrile Powder and Crumb Elastomer Nipol 1432T is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile content. Sufficient antioxidant is added during manufacture for normal storage conditions.Used in adhesives and.. |
|||
Glass Transition Temp, Tg | -35.0 - -25.0 °C | -31.0 - -13.0 °F | |
Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer Nipol 1442 is a copolymer of butadiene and acrylonitrile with medium-high acrylonitrile content. Nipol 1442 shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5%mi.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | DSC |
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.Features: Very tough, high modulus, high tear and tensile properties t.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | 10°C/min |
Covestro Texin® 4210 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | 10°C/min |
Covestro Texin® 4215 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | DSC, 10°C/min (inf); DuPont Test |
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | Cured property; ASTM E831-86 |
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component.. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -35.0 °C | -31.0 °F | Pellet sample |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |