Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 56 %
56 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Users viewing this material also viewed the following: