Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 110 °C | 230 °F | |
NextGen Adhesives G907-08 Epoxy Adhesive Description: NGAC G907-08 is a low viscosity, electrically insulating, heat cured and 2-part adhesive systems designed for applications where temperature and chemical resistance is critical. The NGA.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
NextGen Adhesives G907-21 Structural Epoxy Adhesive Description: NGAC G907-21 is a high viscosity and thixotropic adhesive system that is specifically formulated for structural bonding applications: industrial, electronics and aerospace.Advantages an.. |
|||
Glass Transition Temp, Tg | 110 - 165 °C | 230 - 329 °F | Average value: 151 °C Grade Count:5 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
Eastman Tenite 383A-08 Cellulose Acetate Propionate
(discontinued **) 8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | ASTM D3418 |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | Ultimate Tg |
Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This .. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | Ultimate Tg |
Tra-Con Tra-Bond 2230 Color Keyed, High Temperature Epoxy Adhesive TRA-BOND 2230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | Ultimate Tg |
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable .. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | Ultimate Tg |
Tra-Con Tra-Bond F230 Color Keyed High Temperature Epoxy Adhesive TRA-BOND F230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Glass Transition Temp, Tg | 110 - 120 °C | 230 - 248 °F | DMA |
Hexcel® HexPly® 1454 125°C Curing Epoxy Matrix HexPly® 1454 is a self-extinguishing epoxy resin system with very high self adhesion properties. It has good handling and is tolerant of a wide range of processing conditions. HexPly® 1454 is idea.. |
|||
Glass Transition Temp, Tg | 110 - 120 °C | 230 - 248 °F | DAN 432 |
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix The HexPly® 174 family is a range of flexible 120°C curing matrix systems for a wide variety of industrial applications and is ideally matched to the following processes: shrink wrap tape, vacuum .. |
|||
Glass Transition Temp, Tg | 110 - 130 °C | 230 - 266 °F | DMA |
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix HexPly® M14 is a modified epoxy resin which provides good adhesion to honeycomb and foam cores. Its self-extinguishing characteristics meet the fire, smoke, and toxicity requirements of aerospace a.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | DSC |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding... |
|||
Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—250°C @ 20°C/Min |
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d.. |
|||
Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—250°C @ 20°C/Min |
Epoxy Technology EPO-TEK® H31D-LV Epoxy Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i.. |
|||
Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—250°C @ 20°C/Min |
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
Epoxyset Epoxibond EB-119SP Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
Atom Adhesives AA-BOND 2123 Epoxy Adhesive AA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. AA-BON.. |
|||
Glass Transition Temp, Tg | 110 °C | 230 °F | |
Atom Adhesives AA-BOND 2153 Epoxy Adhesive AA-BOND 2153 is a thixotropic (smooth paste) thermal conductive epoxy system that passes the NASA Outgassing Specification. It is used for staking transistors, diodes, resistors, integrated circuits.. |