Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET
(Unverified Data**) Hytrel® HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal durometer hardness of 45D, is pigmented black with fine particle size carbon black an.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Mallard Creek Polymers ROVENE® 6050 Acrylic Emulsion ROVENE® 6050 is a very soft acrylic latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight allows the formulation of permanent label.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Mallard Creek Polymers Rovene® 6104 Resin Supported Emulsion Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Mallard Creek Polymers ROVENE® 97982 Acrylic Emulsion ROVENE® 97982 is a very soft acrylic latex emulsion suggested as a base resin in flexible packaging laminating adhesives. Rovene® 97982 provides formulations with excellent clarity and UV stab.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
LG Chemical LC180 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear application.Application: Polymer modification, Shoe sole, Film coe.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC, 50°F/min; DIN 51.007 |
Lubrizol Advanced Materials Pearlthane® Maxi 12T85E Thermoplastic Polyurethane Elastomer PEARLTHANE® MAXI 12T85E is a polyester based TPU, supplied in form of transparent, colorless pellets, featuring medium hardness, good mechanical properties and outstanding abrasion resistance. Th.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® U0251M Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® U101 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Styron XZ 94462.04 Carboxylated SB Performance Features: Very soft tacky filmApplications: Fiber Binding and NonwovensEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, .. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | ExxonMobil Method |
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC, 10°C/min (inf); DuPont Test |
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC, 10°C/min (inf); DuPont Test |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |
|||
Glass Transition Temp, Tg | -45.0 °C | -49.0 °F | DSC |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |