Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa and IndiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78

@Time 5.00 sec
72 - 78

@Time 0.00139 hour
ASTM D2240
Tensile Strength 48.3 MPa
7010 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
300% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Tear Strength 17.5 kN/m
100 pli
Trouser; ASTM D470
Graves Tear Strength 68.4 kN/m
390 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 21
21
H18, 1000g; ASTM D3389
Tensile Set 4.0 %
4.0 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Processing Properties Metric English Comments
Zone 1 177 °C
351 °F
Extrusion
Zone 2 182 °C
360 °F
Extrusion
Zone 3 188 °C
370 °F
Extrusion
Zone 4 194 °C
381 °F
Extrusion
Adapter Temperature 194 °C
381 °F
Extrusion
Die Temperature 194 °C
381 °F
Zone 1, Extrusion
194 °C
381 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C