Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LC180 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LC180 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear application.Application: Polymer modification, Shoe sole, Film coextrusionCSA No. 26221-73-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.885 g/cc
0.885 g/cc
ASTM D1505
Mooney Viscosity 20

@Temperature 121 °C
20

@Temperature 250 °F
1+4(121); ASTM D1646
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength at Break 17.3 MPa
2510 psi
ASTM D638
Elongation at Break 670 %
670 %
ASTM D638
1% Secant Modulus 29.7 MPa
4310 psi
ASTM D790
Tear Strength 58.0 kN/m
331 pli
Type C; ASTM D624
Thermal Properties Metric English Comments
Melting Point 73.0 °C
163 °F
Glass Transition Temp, Tg -45.0 °C
-49.0 °F