Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.70 - 1.77 J/g-°C | 0.406 - 0.423 BTU/lb-°F | Average value: 1.72 J/g-°C Grade Count:8 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1600 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 2000 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1895 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Bayblend® KU 2-1514* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeball indentation temperature =125 °CVicat/B 120 temperature = 136 °CUL-listing 94 V-0 at 1.5 mmsuitable for supporting life componen.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® 3385A Polyurethane Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 5080A Polyurethane injection molding gradeimproved microbial resistanceImproved hydrolysis resistanceApplicationSealsmembraneshard - soft systemsPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 8798A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9659DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9665DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPneuma.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® W DP 89051D Polyurethane PreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2467 Polycarbonate ISO 7391-PC,MFLR,(,,)-18-9Global gradeFormerly Makrolon DP1-1870MVR (300 °C/1.2 kg) 19 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmLow viscosityUV stabilizedEasy r.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® Rx2530 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 .. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® A3W PA66 (Conditioned) Description: Free-flowing, heat aging resistant and rapidly processable grade for technical parts subject to high stress such as bearings and bearing cages, gearwheels and spool bodies.Information p.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® B3K BK00464 PA6 (Conditioned) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |