Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5621Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5640Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2179 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FE-5642Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FG-5630Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | Melt |
Covestro Bayblend® T88 GF-10* Polycarbonate + SAN Glass Filled Impact Grade Developmental productInjection molding grade10 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 5100 MPaVicat/B 120 = 134 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | Melt |
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled Injection molding grade10 % glass fiber filledtensile modulus = 3900 MPaVicat/B 120 temperature = 131 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl .. |
|||
Specific Heat Capacity | 1.65 - 1.67 J/g-°C | 0.394 - 0.399 BTU/lb-°F | Average value: 1.65 J/g-°C Grade Count:40 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Specific Heat Capacity | 1.65 J/g-°C | 0.394 BTU/lb-°F | |
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |