Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C @Temperature 100 °C |
0.359 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 1.50 J/g-°C @Temperature 100 °C |
0.359 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 1.50 J/g-°C @Temperature 100 °C |
0.359 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **) Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Average value: 1.50 J/g-°C Grade Count:14 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Specific Heat Capacity | 1.50 - 1.90 J/g-°C | 0.359 - 0.454 BTU/lb-°F | Average value: 1.80 J/g-°C Grade Count:5 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | liquid |
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe POM Copolymer Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |