Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | Average value: 1.46 J/g-°C Grade Count:9 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Specific Heat Capacity | 1.46 - 1.50 J/g-°C | 0.349 - 0.359 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:9 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV8112 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DEBT (deputy tin deflagrate) as the stan.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast UF4 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.350 BTU/lb-°F | |
Trelleborg AEM Syntac® Eccolite® Ultra Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robus.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Asahi Kasei Delpet® 560F Acrylic Molding Compound 560F has the highest flow of Delpet® grades, allowing reduced screw load for broad selection of molding conditions. General Delpet® qualities include attractive transparency, elegant luster and c.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade 80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar.. |
|||
Specific Heat Capacity | 1.46 J/g-°C @Temperature 25.0 °C |
0.350 BTU/lb-°F @Temperature 77.0 °F |
Dupont 900 (Therm. An. Cal.) |
Spartech Polycast Poly FR9 (0.060") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |