Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM E1269 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:5 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:33 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |