Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 0% cold reduction
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 20% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, sheet, 32 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 400 °C
0.129 BTU/lb-°F

@Temperature 752 °F
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 0% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 0% cold reduction, 1065°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 10% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 10% cold reduction, 1010°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 10% cold reduction, 1121°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 50% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, all-weld metal GTAW
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar after 16000 hours at 537°C
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar after 16000 hours at 648°C
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar, after 0 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar, after 4000 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar, after 8000 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar, after 8000 hours at 760°C (1400°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, bar, after 8000 hours at 870°C (1600°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, sheet after 1000 hours at 760°C (1400°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 20% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, sheet after 1000 hours at 871°C (1600°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Specific Heat Capacity 0.538 J/g-°C

@Temperature 500 °C
0.129 BTU/lb-°F

@Temperature 932 °F
Haynes 556® alloy, 40% cold reduction, 1065°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..