Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 220 - 275 °C | 428 - 527 °F | Average value: 259 °C Grade Count:64 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Melting Point | 214 - 275 °C | 417 - 527 °F | |
Johnson Matthey LM10A Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 652 Nylon 6/6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 623 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 605 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 631 Nylon 6/6, Glass Reinforced, Flow Enhanced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 684 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 633 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 637 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 656 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 62S1 Internally Lubricated, Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |