Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 162 - 180 °C | 324 - 356 °F | Average value: 173 °C Grade Count:3 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melting Point | 160 - 180 °C | 320 - 356 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P.. |
|||
Melting Point | 170 - 180 °C | 338 - 356 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
Melting Point | 116 - 180 °C | 240 - 356 °F | Average value: 161 °C Grade Count:117 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Melting Point | 165 - 180 °C | 329 - 356 °F | ASTM D3418 |
3M Dyneon™ THV™ 500 Fluorothermoplastic
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Melting Point | 150 - 180 °C | 302 - 356 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Melting Point | 160 - 180 °C | 320 - 356 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Melting Point | 96.0 - 180 °C | 205 - 356 °F | |
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9270 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 166 - 180 °C | 331 - 356 °F | ASTM D3418 |
BiologiQ EcoStarch GS270 Thermoplastic Starch BiologiQ GS270 is a plasticized thermoplastic starch (TPS) called EcoStarch Resin (ESR). It is suitable for blending with petrochemical or bioresins where biobased content is desired. It Can be us.. |
|||
Melting Point | 162 - 180 °C | 324 - 356 °F | Average value: 172 °C Grade Count:11 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9255 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |