Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4... |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 53% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1315 - 1440 °C | 2399 - 2620 °F | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |