Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 343 °C | 649 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Melting Point | 343 °C | 649 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 150P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® Pipes™ PEEK polymer VICTREX Pipes™ are durable, lightweight pipe and tube extruded from VICTREX® PEEK polymer which offer high temperature performance and a unique combination of properties. An excellent alternative .. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Victrex® Vicote® F817 Polyetheretherketone (PEEK) Liquid Dispersion, Enhanced Adhesion Grade Vicote F817 can be applied to most ferrous and non ferrous metals. Cast metals need to be de-gassed in an oven to prevent pin holes in the coating surface. Aluminum and other thermal sensitive subst.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Melting Point | 343 °C | 649 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Melting Point | 343 °C | 649 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-107 Compression Molded PEEK Compound, 25% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-109 Compression Molded PEEK Compound, 30% Carbon Fiber with 15% PTFE Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-115 Compression Molded PEEK Compound, Static Dissipative Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-118 Compression Molded PEEK Compound, 20% Fiberglass with 5% PTFE Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | DSC |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Melting Point | 343 °C | 649 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced PEEKInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Melting Point | 343 °C | 649 °F | ISO 11357 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |