Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F817 Polyetheretherketone (PEEK) Liquid Dispersion, Enhanced Adhesion Grade

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Victrex® Vicote® F817 Polyetheretherketone (PEEK) Liquid Dispersion, Enhanced Adhesion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vicote F817 can be applied to most ferrous and non ferrous metals. Cast metals need to be de-gassed in an oven to prevent pin holes in the coating surface. Aluminum and other thermal sensitive substrates may be coated however the mechanical properties of the substrate may be affected. F817 can be used on metal substrates where limited surface roughening is allowed or desired. Complies with FDA 21 CFR 175.300Information Provided by VICTREX®
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc

@Temperature 25.0 °C
1.15 g/cc

@Temperature 77.0 °F
ISO 2811
Solids Content 28 %
28 %
theory volume
40 %
40 %
weight; Victrex Internal Test Method
pH 10
10
Victrex Internal Test Method
Viscosity Measurement 30
30
[seconds]; Test Method: BS EN ISO 2431 Din 6 Cup; @ 25°C
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 1kg, Indent 15mm; ISO 6772
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Conical Blend pass at 3mm
ISO 6860
Konig Hardness (seconds) 118
Test Method: BS EN ISO 1522