Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 232 °C
450 °F
Indium Corp. Indalloy 128 Pure Tin
Information Provided by Indium Corporation
Melting Point 232 - 345 °C
450 - 653 °F
Indium Corp. Indalloy 173 Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 232 - 235 °C
450 - 455 °F
Indium Corp. Indalloy® 129 99Sn/1Sb Lead-Free Solder Alloy
Information provided by the manufacturer, Indium Corporation.
Melting Point 232 - 238 °C
450 - 460 °F
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy
Information provided by the manufacturer, Indium Corporation.
Melting Point 232 - 248 °C
450 - 478 °F
Limits; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ Plus 1111 PET Resin
Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un..
Melting Point 232 - 248 °C
450 - 478 °F
Limits; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ Refresh 1101 PET Resin
Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen..
Melting Point 232 °C
450 °F
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
Melting Point 232 °C
450 °F
Williams Advanced Alloys WS232 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 232 - 238 °C
450 - 460 °F
Williams Advanced Alloys WS238A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 232 - 240 °C
450 - 464 °F
Williams Advanced Alloys WS240 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 232 °C
450 °F
DSC Peak; JIS K7121
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Melting Point 232 °C
450 °F
ChevronTexaco Amber Petrolatum
Chevron Petrolatums are ash-free mixtures of mineral oils and a special petroleum wax with a smooth grease-like texture.ApplicationsChevron Petrolatums find wide use in pharmasutical and cosmetic pr..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin
Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin
Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin
Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel ..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel ..
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Ant..
Melting Point 232 °C
450 °F
ChevronTexaco Snow White Petrolatum, Snow White
Chevron Petrolatums are ash-free mixtures of mineral oils and a special petroleum wax with a smooth grease-like texture.ApplicationsChevron Petrolatums find wide use in pharmasutical and cosmetic pr..
Melting Point 232 °C
450 °F
10 K/min
BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET
Melting Point 232 - 249 °C
450 - 480 °F
ASTM D789
Adell WR-37 33% Glass Reinforced PET
Melting Point 232 - 268 °C
450 - 514 °F
Average value: 251 °C Grade Count:20
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Melting Point 232 - 249 °C
450 - 480 °F
ASTM D789
Adell WL-38 40% Glass and Mineral Reinforced PET