Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 167 °C | 333 °F | (10°C/min); ISO 11357-1,2,3 |
Aardvark Polymers AARTEL® 800AM Rotational Molding Resin Aartel 800AM is a new antimicrobial grade that offers the same excellent physical and mechanical properties of standard Aartel grades plus the added benefit of protection against microbial growth, p.. |
|||
Melting Point | 167 °C | 333 °F | ISO 11357 |
Polyram RamOfin PPH501G4 Polypropylene, 20% Glass Fiber, Flame Retardant Glass fiber 20% reinforced, halogen free, flame retardant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 HI2 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 TF2 POM Tribological modified grade with addition of 10% PTFE, which causes decreased coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 XEC1 POM Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe .. |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 400 POM Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 167 °C | 333 °F | 10 K/min |
BASF Ultraform W 2320 003 BK120 Q600 POM Ultraform W 2320 003 BK120 Q600 is a pigmented black, very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties .. |
|||
Melting Point | 167 °C | 333 °F | ISO 11357-1/-3 |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Melting Point | 167 °C | 333 °F | DIN 53765 |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Melting Point | 167 °C | 333 °F | |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Melting Point | 167 °C | 333 °F | ISO 11357-1/-3 |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Melting Point | 167 °C | 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 GB4 POM 20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 167 °C | 333 °F | DIN 53765 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Melting Point | 167 °C | 333 °F | ISO 11357-1/-3 |
BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |
|||
Melting Point | 167 °C | 333 °F | ISO 11357-1/-3 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Melting Point | 167 °C | 333 °F | |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |