Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 135 °C | 275 °F | STN EN 11357-1 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Melting Point | 135 °C | 275 °F | |
Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retar.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Multi-color OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, 589 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, AB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, F-Ex OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SGB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding Eraclene MR 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MR 80 shows a good balance between processability and mechanical p.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 400 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 620 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | MTM 15902 |
LyondellBasell Adsylâ„¢ 5 C 37 F Polyolefin Description: Adsylâ„¢ 5 C 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an.. |
|||
Melting Point | 135 °C | 275 °F | MTM 15902 |
LyondellBasell Adsylâ„¢ 5 X 37 F Polyolefin Description: Adsylâ„¢ 5 X 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a relatively high.. |
|||
Melting Point | 135 °C | 275 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL6013T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 135 - 145 °C | 275 - 293 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM30 30% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 135 °C | 275 °F | ASTM D-3418 |
Saint-Gobain Norton® UHMW PE Skived PTFE Film Description: UHMWPE = ultra-high molecular weight polyethylene; PTFE = polytetrafluoroethyleneApplications include: Common in Protective/Decorative ApplicationsInformation provided by Saint Gobain P.. |
|||
Melting Point | 135 °C | 275 °F | ISO 11357 |
Total HDPE HL 717 High Density Polyethylene - Blown Film HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It.. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | |
Addcomp PRIEX® Ionomer 48101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |
|||
Melting Point | 135 - 138 °C | 275 - 280 °F | ASTM D789 |
Rochling Engineered Plastics Polystone® Reprocessed (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® EST-8 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |