Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Flexirene® MS 40 U Linear Low Density Polyethylene Flexirene MS 40 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 40 U are characterized by a good balance be.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5202.09 Compounding Resin
(discontinued **) LL 5202.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL 5202.09 makes for efficient blending with pigments, slip .. |
|||
Melting Point | 123 °C | 253 °F | ASTM D3418 |
ExxonMobil LL 6202 Injection Molding Resin
(discontinued **) LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear.. |
|||
Melting Point | 123 °C | 253 °F | Exxon Method |
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all.. |
|||
Melting Point | 123 °C | 253 °F | ISO 11357 |
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1002.09 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1107x95 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melting Point | 123 °C | 253 °F | ASTM D3418 |
ExxonMobil LL 6202.19 Injection Molding Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ELITE™ 5110G Enhanced Polyethylene Resin ™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applicatio.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid DOW GRSN-9820 NT 7 is produced using UNIPOL™ PE process technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other master .. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Melting Point | 123 - 129 °C | 253 - 264 °F | Average value: 127 °C Grade Count:8 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have.. |