Polymer Property : Melting Point = 185 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 85.0 - 125 °C
185 - 257 °F
S&E Specialty Polymers GPE2001E-ROHS PVC
GPE2001E-ROHS flame retardant polyethylene compound designed for wire and cable applications. GPE2001E-ROHS complies with RoHS requirements. GPE2001E-ROHS is suitable for 75°C continuous use and 10..
Melting Point 85.0 - 125 °C
185 - 257 °F
S&E Specialty Polymers GPE2001F-ROHS PVC
Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont..
Melting Point 85.0 °C
185 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio..
Melting Point 85.0 °C
185 °F
Upon Melting via DSC/ASTM D3418
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin  (discontinued **)
Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc..
Melting Point 85.0 °C
185 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 85.0 °C
185 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 85.0 °C
185 °F
Exxon Method
ExxonMobil Escorene® LD-720 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p..
Melting Point 85.0 °C
185 °F
Exxon Method
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App..
Melting Point 85.0 °C
185 °F
Exxon Method
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..
Melting Point 85.0 °C
185 °F
TRN-14
Tipco Tipcolite® TPF 1110 - Unreinforced Thermoset Phenolic Resin, 40mm Norton Flow with 9% Hexamine
Unreinforced Phenolic Resin having 40mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Melting Point 85.0 °C
185 °F
TRN-14
Tipco Tipcolite® TPF 550 - Unreinforced Phenolic Resin having 41 mm Norton Flow with 9% Hexamine
Unreinforced Phenolic Resin having 41mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd., Ind..
Melting Point 85.0 °C
185 °F
DSC Peak; D33418
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength ..
Melting Point 85.0 °C
185 °F
DSC Peak; ASTM D3418
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength..
Melting Point 85.0 °C
185 °F
Peak, by DSC; ASTM D3418
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer
Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s..
Melting Point 85.0 °C
185 °F
DSC Peak; D33418
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal ..
Melting Point 85.0 °C
185 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion ..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 °C
185 °F
ASTM D3418, ISO 3146
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Melting Point 85.0 °C
185 °F
D.S.C. method
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Melting Point 85.0 °C
185 °F
DSC
Arkema Group BONDINE® HX 8290 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
BONDINE® HX 8290 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. This grade is characterised by a high fluidity. Due..
Melting Point 85.0 °C
185 °F
Exxon Method
ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams..
Melting Point 85.0 °C
185 °F
Exxon Method
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..
Melting Point 85.0 °C
185 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..