Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Oceanchem Group Decabromodiphenyl Oxide (DECA/DBDPO) Molecular Formula: C12Br10OCas No.: 1163-19-5Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: It is .. |
|||
Melting Point | 288 - 310 °C | 550 - 590 °F | |
PolyOne Trilliant™ HC HC3220-0030 RS Natural Polycarbonate (PC) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Melting Point | 227 - 310 °C | 441 - 590 °F | |
Nihon Superior SN100C3 High Temperature Dipper and Tinning Solder High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | ASTM D4591 |
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antist.. |
|||
Melting Point | 200 - 310 °C | 392 - 590 °F | Average value: 260 °C Grade Count:44 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Melting Point | 235 - 310 °C | 455 - 590 °F | Average value: 258 °C Grade Count:38 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Melting Point | 290 - 310 °C | 554 - 590 °F | |
Indium Corp. Indalloy 12 Lead Solder Alloy Tin-free indium solderInformation Provided by Indium Corporation |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P7310 Perfluoroalkoxy (PFA) Hyflon® PFA P7310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 302 - 310 °C | 575 - 590 °F | ASTM D-3418 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Melting Point | 302 - 310 °C | 576 - 590 °F | |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Melting Point | 302 - 310 °C | 576 - 590 °F | |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Melting Point | 302 - 310 °C | 576 - 590 °F | |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Melting Point | 302 - 310 °C | 576 - 590 °F | |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Melting Point | 302 - 310 °C | 576 - 590 °F | |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |