Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC300BF Polypropylene Homopolymer for Capacitor Film Borclean HC300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC300BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC314BF Polypropylene Homopolymer for Capacitor Film Borclean HC314BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC314BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film Borclean HC318BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC318BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC320BF Polypropylene Homopolymer for Capacitor Film Borclean HC320BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC320BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borflow™ HL504FB Polypropylene Homopolymer Borflow HL504FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product .. |
|||
Melting Point | 162 - 165 °C | 324 - 329 °F | ISO 3146 |
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HF420FB Polypropylene HF420FB is a polypropylene homopolymer intended for fiber applications. HF420FB has been developed especially for applications like: staple fiber, continuous filaments, and spun bonded nonwovens.In.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HG455FB Polypropylene Homopolymer HG455FB is a polypropylene homopolymer intended for fiber applications. Applications: fine filament count at high spinning speeds, spun bonded nonwovens, and POY production.Information provided by .. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 5724 Polypropylene, Extra High Impact Copolymer ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 4720 WZ Polypropylene, Impact Copolymer ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4944CWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffnes.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 4944WZ Polypropylene, Impact Copolymer ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP10 GR10 NL PPCP, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP10 GR30 NL PPCP, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Melting Point | 135 - 165 °C | 275 - 329 °F | Average value: 157 °C Grade Count:8 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |