Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 85.0 - 125 °C | 185 - 257 °F | |
S&E Specialty Polymers GPE2001E-ROHS PVC GPE2001E-ROHS flame retardant polyethylene compound designed for wire and cable applications. GPE2001E-ROHS complies with RoHS requirements. GPE2001E-ROHS is suitable for 75°C continuous use and 10.. |
|||
Melting Point | 85.0 - 125 °C | 185 - 257 °F | |
S&E Specialty Polymers GPE2001F-ROHS PVC Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont.. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melting Point | 85.0 °C | 185 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Melting Point | 85.0 °C | 185 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 85.0 °C | 185 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 720.92 Specialty Film Resin
(discontinued **) Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-720 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Melting Point | 85.0 °C | 185 °F | TRN-14 |
Tipco Tipcolite® TPF 1110 - Unreinforced Thermoset Phenolic Resin, 40mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 40mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; D33418 |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; ASTM D3418 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Melting Point | 85.0 °C | 185 °F | Peak, by DSC; ASTM D3418 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |
|||
Melting Point | 85.0 °C | 185 °F | DSC Peak; D33418 |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
Melting Point | 85.0 °C | 185 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 - 95.0 °C | 185 - 203 °F | DSC |
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 85.0 °C | 185 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A.. |
|||
Melting Point | 85.0 °C | 185 °F | D.S.C. method |
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Melting Point | 85.0 °C | 185 °F | DSC |
Arkema Group BONDINE® HX 8290 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride BONDINE® HX 8290 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. This grade is characterised by a high fluidity. Due.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Melting Point | 85.0 °C | 185 °F | Exxon Method |
ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Melting Point | 85.0 °C | 185 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |