Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 175 °C | 347 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Melting Point | 175 °C | 347 °F | DSC, both heating and cooling speeds of 10°C/min |
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, .. |
|||
Melting Point | 175 °C | 347 °F | DSC |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Melting Point | 175 - 178 °C | 347 - 352 °F | Average value: 177 °C Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melting Point | 175 - 188 °C | 347 - 370 °F | Huntsman/TMA |
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | |
Williams Advanced Alloys WS187 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram PlusTek PD300G4 Nylon 12, 20% Glass Fiber 20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | <= 175 °C | <= 347 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv.. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM) Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over .. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM) Delrin® 507 is a general purpose homopolymer acetal containing a UV stabilizer ideally suited for outdoor applications or those in which there is an otherwise abundant source of UV light.General hi.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part .. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |
|||
Melting Point | 175 °C | 347 °F | |
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM) Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep.. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Dry) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Melting Point | 175 °C | 347 °F | (Dry) |
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading .. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Adamas Lakinor® U PVDF Information provided by Adamas, HPM |
|||
Melting Point | 175 °C | 347 °F | (Dry) |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |