Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 174 °C | 345 °F | ASTM D3418 |
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
3M Dyneon™ PVDF 1010/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melting Point | 174 - 184 °C | 345 - 363 °F | Average value: 177 °C Grade Count:9 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 174 - 178 °C | 345 - 352 °F | Average value: 175 °C Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melting Point | 174 - 186 °C | 345 - 367 °F | |
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy Pb free solder. Zn causes high drossing; corrosion concerns.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
SK Chemicals SKYPEL G130D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | <= 174 °C | <= 345 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 02020 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 02020 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 02020 is an excellent sealing materi.. |
|||
Melting Point | <= 174 °C | <= 345 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 02020 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02020 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12 Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 20 X PA12-I Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Dry) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. Good chemical resistance. Very good ability .. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent... |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |