Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 138 °C | 280 °F | |
Multibase Multi-Flex® TPE D 4502 BLK Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo.. |
|||
Melting Point | 138 °C | 280 °F | |
Multibase Multi-Flex® TPO D 4508 D 4508 This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase. |
|||
Melting Point | 138 °C | 280 °F | Flow temperature, ASTM D569-59 |
Rotuba 860MS 686.5 Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 138 °C | 280 °F | Internal method |
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling... |
|||
Melting Point | 138 °C | 280 °F | Flow temperature, ASTM D569 |
Rotuba MSS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 138 - 148 °C | 280 - 298 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |
|||
Melting Point | 138 °C | 280 °F | Flow temperature; ASTM D569 |
Plaskolite Optix® PL-150 Acrylic Resin
(discontinued **) Injection/extrusion pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Melting Point | 138 °C | 280 °F | |
Hong Kun Group UV 326 UV Absorber UV-326 is a important ultraviolet absorber of bonzotriazoleseries, which is stable, nontoxic, higher absorbency for ultraviolet ray. Widely used for photosensitive materials and poly merized materia.. |
|||
Melting Point | 138 °C | 280 °F | |
Hyosung Topilene C600MU PP C600MU Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 138 °C | 280 °F | Eutectic |
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m.. |
|||
Melting Point | 138 - 148 °C | 280 - 298 °F | |
Fine Organics FINAWAX C Lubricant Additive Applications: Antiblock agent for soft PVC films/sheets, strong release agent for rigid PVC calendered sheets, dispersant for FRLS PVC compounds.Information provided by Fine Organics |
|||
Melting Point | 138 - 170 °C | 280 - 338 °F | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 138 - 150 °C | 280 - 302 °F | |
Struktol TR EBS Processing Additive, Dispersant N,N` Ethylene Bis-stearamideSTRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carri.. |
|||
Melting Point | 138 - 144 °C | 280 - 291 °F | ISO 3146 |
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film Borclear RD738CF is a slip and antiblock formulation propylene alpha olefin copolymer resin. It is suitable for the manufacturing of unoriented film on chill roll process.Borclear RD738CF is suitabl.. |
|||
Melting Point | 138 - 144 °C | 280 - 291 °F | ISO 3146 |
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | ISO 3146 |
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | DSC; ISO 3146 |
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | ISO 3146 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |
|||
Melting Point | 138 - 154 °C | 280 - 310 °F | |
DayGlo ZQ Pigments ZQ-18 Signal Green DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 138 - 154 °C | 280 - 310 °F | |
DayGlo ZQ Pigments ZQ-19 Horizon Blue DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 138 - 170 °C | 280 - 338 °F | |
AIM 40Bi/60Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 138 - 170 °C | 280 - 338 °F | |
AIM 54Sn/26Pb/20In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 138 °C | 280 °F | |
AIM 58Bi/42Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | >= 138 °C | >= 280 °F | |
Oceanchem Group Hydroxymethylphenylphosphinic Acid (HMPPA) Molecular Formula: C7H9O3PCas No.: 61451-78-3Application: HMPPA is a bifunctional copolymerisable phosphorous flame retardant monomer, which can be polycondesated with ethylene glycol and terephthal.. |
|||
Melting Point | <= 138 °C | <= 280 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 0433EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: .. |
|||
Melting Point | 138 °C | 280 °F | Peak; DSC |
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene Product Description: Exxelor Po 1015 polymer resin is a maleic anhydride fuctionalized polypropylene copolymer, produced by reactive extrusion. It has been primarily designed to add polarity to poly.. |
|||
Melting Point | 138 - 175 °C | 280 - 347 °F | Average value: 155 °C Grade Count:9 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |