Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, 589 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, DryRun OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, Q OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SGB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding Eraclene MR 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MR 80 shows a good balance between processability and mechanical p.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Melting Point | 135 °C | 275 °F | |
Plastcom SLOVALEN PC 93 T 15 1/M PP, 15% mineral filling, UV stability FeaturesModified PP for injection moulding with the content of 15 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Melting Point | 135 - 138 °C | 275 - 280 °F | ASTM D789 |
Rochling Engineered Plastics Polystone® Natural (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, CL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 400 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | |
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Melting Point | 135 °C | 275 °F | MTM 15902 |
LyondellBasell Adsylâ„¢ 5 C 39 F Polyolefin Description: Adsylâ„¢ 5 C 39 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an.. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and .. |
|||
Melting Point | 135 °C | 275 °F | |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Melting Point | 135 °C | 275 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Melting Point | 135 °C | 275 °F | 10°C/min |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 135 - 145 °C | 275 - 293 °F | Sheath |
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib.. |