Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 - REG PE Multicoloured coarse OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, UV - stabilized OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 °C | 271 °F | Petromont |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Melting Point | 133 °C | 271 °F | Petromont |
Petromont 2200 High Density Polyethylene Resin Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr.. |
|||
Melting Point | 133 - 138 °C | 271 - 280 °F | |
Polikim ULPOLEN® 1000 UHMWPE, Oil The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner.. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 - REG PE Multicoloured fine OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 °C | 271 °F | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Melting Point | 133 °C | 271 °F | |
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade Easy-to-process blow molding grade for stackable canisters (up to 60 l), used for packing surface-active liquids, laundry and dishwashing detergents, disinfectants, drums (up to 220 l) for various s.. |
|||
Melting Point | 133 °C | 271 °F | |
Hyosung Topilene C600ME PP C600ME Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 133 °C | 271 °F | DSC |
LG Chemical LUTENE-H FE0070 HDPE LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b.. |
|||
Melting Point | 133 °C | 271 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC PB283 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | |
Hong Kun Group 5-(Chloromethyl)-2-Methylpyridine Hydrochloride Pharmaceutical Intermediate Chemical Name: Pyridine, 5-(chloromethyl)-2-methyl, hydrochloride (9Cl)Formula: C7H9Cl2NSynonymy: 6-methyl-3-chloromethyl pyridine hydrochloride2-Methylpyridine-5-Chloromethyl Hydrochloride6-Methyl-.. |
|||
Melting Point | 133 °C | 271 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H6007JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh rigidityHigh impact resistanceGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drink, bottles, pallet, garbage bins, con.. |
|||
Melting Point | 133 °C | 271 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, .. |
|||
Melting Point | 133 - 136 °C | 271 - 277 °F | ISO 3146 |
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal.. |
|||
Melting Point | 133 °C | 271 °F | ISO 11357-3 |
Borealis FS1560 High Density Polyethylene FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala.. |
|||
Melting Point | 133 °C | 271 °F | ISO 11357 |
Polyram Bondyram® 5108 Maleic Anhydride Modified High Density Polyethylene Recommended for coupling of glass and Halogen free fillers in PE composites.Information provided by Polyram. |
|||
Melting Point | 133 °C | 271 °F | |
Unitika elitel UE3800 Polyester, Pellet Hot melt adhesives, Adhesives for polyvinylchlorideUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesiv.. |
|||
Melting Point | 133 °C | 271 °F | ISO 11357 |
Total HDPE HD 6081 High Density Polyethylene - Injection Molding HD 6081 is a high density polyethylene with very good organoleptic properties, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by .. |
|||
Melting Point | 133 °C | 271 °F | ISO 11357 |
Total Lumicene® M6040 Metallocene High Density Polyethylene Lumicene® M6040 is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, rigidity and processability.It is especially suited for t.. |
|||
Melting Point | 133 °C | 271 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula.. |
|||
Melting Point | 133 °C | 271 °F | Exxon Method |
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula.. |