Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E 28 |
Micropol E332 Rotational molding powder based on a random EVA copolymer Information provided by Micropol Limited |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
DuPont Elvax® 150 Ethylene Vinyl Acetate DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
DuPont Elvax® 150W Ethylene Vinyl Acetate DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
DuPont Elvax® 240W Ethylene Vinyl Acetate DuPont™ Elvax® 240W is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 240W resins can be used for the following applications.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
Westlake Epolene® C-13 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-13 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color con.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
Westlake Epolene® N-30 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-30 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
Arkema Group LOTRYL® 35 BA 40 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 40 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 40 is particularly r.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
DuPont Elvax® 240 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants,.. |
|||
Ring & Ball Softening Point | 110 °C | 230 °F | ASTM E28 |
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th.. |