Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -20.0 - 150 °C |
9.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 G/C40 L UV 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedTPCI# 6024102Informa.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 HS UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L UV BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 RM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low Moisture AbsorptionAppearance: BlackTPCI# 9719102Information provided by T.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 UV BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearan.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 HS L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L NAT004 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 9411102Informatio.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L RD041 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: YellowTPCI# 8221102Information provi.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L RD079 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: RedInformation provided by TP Compos.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 TL20 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE Lubricant (20%) Features: LubricatedAppearance: BlackInformation provided.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 HS Up BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat Sta.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 L NAT024 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 8221102Informatio.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT G/CF30 IM 15% Glass/Carbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInform.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PEI GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |