Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 144 µm/m-°C | 80.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE 8904 UV GY Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 144 µm/m-°C | 80.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 144 µm/m-°C @Temperature 23.0 - 60.0 °C |
80.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East) LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties |
|||
CTE, linear, Parallel to Flow | 144 µm/m-°C | 80.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 144 µm/m-°C | 80.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® HDPE GL5 Availability: North AmericaForms: PelletsAdditive: Graphite Powder LubricantInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 144 µm/m-°C @Temperature 23.0 - 60.0 °C |
80.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP FP003 PE (Europe-Africa-Middle East) LNP *Lubricomp* FP003 is a compound based on Polyethylene resin, containing PTFE and Silicone. Added features include: Internally Lubricated. |