Polymer Property : CTE, linear, Parallel to Flow = 22.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E831
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 0390 BK
Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6/10 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® POM CO GF20 CC 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PP 0123 C Polypropylene
Availability: North AmericaForms: PelletsFeatures: Copolymer and Thermally ConductiveInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Luriblend® PA6/6 04003 Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Luriblend® PA6/6 CF10 TS15 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(13%) and Silicone Lubricant(2%)Features: Lubricated Appearance: BlackInforma..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Statiblend® PBT 03003
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Statiblend® PBT GF10 SS5 MB
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp..
CTE, linear, Parallel to Flow 39.6 - 50.4 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 - 28.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA
10% Glass Reinforced PPE+PA Alloy.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Electrablend® PA6/6 03001 Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PA6 0390 S1 BK
Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® POM CO GF20 UV BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInformati..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File ..
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Techmer ES HiFill® TPX-HTN-03003 A 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightFeatures: Platable and High Temperature StrengthUL File Number: E157318Information provided by TP C..
CTE, linear, Parallel to Flow 39.6 - 50.4 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 - 28.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific)
GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting.
CTE, linear, Parallel to Flow 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PlastxWorld CEVIAN® VGR20 20% GF ABS
Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
CTE, linear, Parallel to Flow 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PlastxWorld CEVIAN®-N GRSJ1 10% GF SAN resin
Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.