Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 50.0 - 150 °C |
13.9 - 19.4 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
CTE, linear, Parallel to Flow | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
CTE, linear, Parallel to Flow | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
CTE, linear, Parallel to Flow | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 20.0 °C |
13.9 - 19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |