Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM1210 PC Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM3110 PC Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM3110R PC Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 60.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 60.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT WM35 X Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® POM CO GF5 CC 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 5% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,.. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® ABS/PBT 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PP CO E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 64.8 µm/m-°C | 36.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PP CO FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi.. |