Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade High-impact grade with good mechanical properties; applications include drawing instruments, scales, containers, display stands; good processing viscosity, especially suitable for coextrusion. Extr.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Polycasa Acryl® KR 2006/1 Acrylic, Impact Grade Impact-modified grade for highly stressed parts; highest impact and notched-impact resistance; can be mixed with general-purpose grades to get the desired toughness; highly resistant to stress crack.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7205 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® XD1507S PBT+PC (Europe-Africa-Middle East) XENOY XD1507S is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties, designed for self coloured, optiwall bumper facias.This data was supplie.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2D 20 nat PA612 Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23 Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |